MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Nickelvac® H-B-2 UNS N10665 Nickel Superalloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Vessels, pumps, valves, piping systems for the production of hydrochloric, sulfuric, acetic, and phosphoric acids.

Property values are for samples in the metallurgical condition: 1600°F age.

Information provided by Allvac, An Allegheny Teledyne Company.

Key Words: ASTM B 333, 335, 622.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.21 g/cc0.333 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9090
Tensile Strength, Ultimate 862 MPa125000 psi
Tensile Strength, Yield 379 MPa
@Strain 0.2 %
55000 psi
@Strain 0.2 %
Elongation at Break 60 %60 %
Reduction of Area 55 %55 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 %0.010 %
Chromium, Cr 0.50 %0.50 %
Cobalt, Co 0.50 %0.50 %
Iron, Fe 1.0 %1.0 %
Manganese, Mn 0.50 %0.50 %
Molybdenum, Mo 16 %16 %
Nickel, Ni 81 %81 %as balance
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.050 %0.050 %
Sulfur, S 0.015 %0.015 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
Special Metals INCONEL® alloy 22 Austenitic Alloy
Special Metals INCONEL® Alloy C-276
Haynes Hastelloy® G-30® alloy, mill annealed
Special Metals INCONEL® Alloy HX

NALLV13 / 14929

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.