Cold rolled carbon steel sheet of structural quality in cut lengths or coils. Moderate ductility. Copper content of 0.20% is a minimum when copper steel is specified.Similar entries in MatWeb include: ASTM A611 grade A, grade C, grade D, grade E |
copper steels, copper-steels |