MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Hysol EA 9380 Paste Adhesive System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Cures at low temperature. Offers strength, toughness and high temperature resistance of heat-curing film adhesives, with greater flexibility and ease of use. Can be applied to large parts with controlled meter mix operation.
    Applications:
  • Structural Repair
  • Composite Bonding
  • Liquid Shim

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 4.00 °C39.2 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 78.0 MPa11300 psi
Compressive Modulus 2.95 GPa428 ksi
Adhesive Bond Strength  >= 24.1 MPa
@Temperature 93.0 °C
>= 3500 psi
@Temperature 199 °F
Tensile Lap Shear
 32.0 MPa
@Temperature -55.0 °C
4640 psi
@Temperature -67.0 °F
Tensile Lap Shear
 37.0 MPa
@Temperature 25.0 °C
5370 psi
@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 9.00 kN/m51.4 pliBell Peel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min
@Temperature 70.0 °C
4.00 hour
@Temperature 158 °F
Pot Life 180 min180 min
 
Descriptive Properties
ConsistencyThixotropic
Form2 parts
Mix Ratio, Part A:Part B100:55
Peel StrengthHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol EA 9360 Paste Adhesive System
Henkel Hysol EA 9377 Paste Adhesive System
Henkel Hysol EA 9330 Paste Adhesive System
Henkel Hysol EA 9394 Paste Adhesive System
Henkel Hysol EA 9359.3 Paste Adhesive System

PHENK814 / 146819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.