MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® W DP89043D Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: injection molding grade; no yellowing under the action of UV light; very good hydrolysis and microbial resistance; good low-temperature flexibility; high rebound resilience; low abrasion; colored applications in the automotive, sports and leisure sectors

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ISO 868
Hardness, Shore D 4343ISO 868
Tensile Strength, Ultimate 30.0 MPa4350 psi200 mm/min; DIN 53504
Tensile Stress at Strain  12.0 MPa
@Strain 100 %
1740 psi
@Strain 100 %
200 mm/min; DIN 53504
 18.0 MPa
@Strain 300 %
2610 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 700 %700 %ISO 527-1/-2
Tensile Modulus  0.101 GPa
@Temperature 60.0 °C
14.6 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.143 GPa
@Temperature 20.0 °C
20.7 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.230 GPa
@Temperature -20.0 °C
33.4 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Flexural Modulus 0.0800 GPa11.6 ksi2 mm/min; ISO 178
Rebound 56 %56 %Resilience; ISO 4662
Tear Strength 96.0 kN/m548 pli500 mm/min; ISO 34-1
Abrasion 1111mm³, Method A; ISO 4649
Compression Set 41 %
@Temperature 70.0 °C
41 %
@Temperature 158 °F
24 hr; ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FInjection
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 85786A Polyurethane
Covestro Desmopan® 487 Thermoplastic Polyurethane
Covestro Desmopan® W DP 85085A Polyurethane
Covestro Desmopan® W DP89056D Polyurethane
Covestro Desmopan® 385 Thermoplastic Polyurethane

PB09829 / 92669

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.