MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Medium Flow

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength, Yield 42.2 MPa
@Thickness 3.20 mm
6120 psi
@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 61.8 MPa
@Thickness 6.40 mm
8960 psi
@Thickness 0.252 in
5 mm/min; ASTM D790
Flexural Modulus 1.86 GPa
@Thickness 6.40 mm
270 ksi
@Thickness 0.252 in
5 mm/min; ASTM D790
Izod Impact, Notched  1.27 J/cm
@Thickness 6.40 mm
2.39 ft-lb/in
@Thickness 0.252 in
ASTM D256
 2.94 J/cm
@Thickness 3.20 mm
5.51 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
@Thickness 6.40 mm
217 °F
@Thickness 0.252 in
Method A; ASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS TS15v04 Injection Molding Grade, ABS/PC Alloy
A. Schulman Diamond DIAMALOY 730 ABS/PC Alloy, Flame Retardant
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy
A. Schulman Diamond ABSPC 7030 ABS/PC Injection Molding Grade, High Impact
A. Schulman Diamond ABSPC 7430-1005T ABS/PC Injection Molding Grade

PBHANS927 / 178095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.