MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Nilcra® Zirconia 3Y-TZP Technical Ceramic
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Yttria-Tetragonal Zirconia Polycrystal (Y-TZP) with excellent transformation toughening properties. ? Comprising 3 mol% (5.2 wt%) Y2O3 in ZrO2 . ? A high purity, fine grain (sub-micron) tetragonal, transformation toughened zirconia (3Y-TZP).

Applications:

  • Typically used for blades and cutting edges where the fine grain structure is an advantageous.
  • Gas and Oil field applications
  • Pump and Valve components
  • Canning and Metal Packaging
  • Solids Handling
  • Automotive (eg Weld Pins)

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.05 g/cc
@Temperature 20.0 °C
0.219 lb/in³
@Temperature 68.0 °F
Grain Size 0.40 µm0.40 µmaverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 13001300kg/mm2
Modulus of Elasticity 205 GPa
@Temperature 20.0 °C
29700 ksi
@Temperature 68.0 °F
Flexural Strength 1000 MPa
@Temperature 20.0 °C
145000 psi
@Temperature 68.0 °F
4 pt bend
Compressive Strength 2300 MPa
@Temperature 20.0 °C
334000 psi
@Temperature 68.0 °F
Poissons Ratio 0.30
@Temperature 20.0 °C
0.30
@Temperature 68.0 °F
Fracture Toughness 10.0 MPa-m½
@Temperature 20.0 °C
9.10 ksi-in½
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+11 ohm-cm
@Temperature 20.0 °C
>= 1.00e+11 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 25.0 - 400 °C
5.00 µin/in-°F
@Temperature 77.0 - 752 °F
Thermal Conductivity 3.00 W/m-K
@Temperature 20.0 °C
20.8 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Other 5.2 %5.2 %Y2zo3 in ZrO2
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
Crucible Steel CPM® 154 Tool Steel
Versalis Extir® EH 3000 Expandable Polystyrene
Zircar Zirconia ZYF-100 Zirconia Felt Insulation

CMORF8059 / 203536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.