MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 9000 - 14000 cP
@Temperature 40.0 °C
9000 - 14000 cP
@Temperature 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 8278 - 82
Tensile Strength at Break 17.16 - 26.97 MPa2489 - 3912 psi
Elongation at Break 510 - 660 %510 - 660 %
Tear Strength 73.5 - 113 kN/m420 - 644 pli
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 °C212 °FWorking Temperature, Prepolymer
Mold Temperature 100 °C212 °F
Pot Life 11 min11 min
 
Descriptive Properties
MOCA Temperature110°C
NCO ContentMax 4%
 Min 3.6%
PHR of MOCA11%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Taiwan PU Corporation CPU-69-A/B Mixing Ratio 100/26 Polyurethane Casting Elastomer
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer
ATG s.r.l. AU-EU Polyurethane Rubber
BCC Products Kwik Kast BC 8001 Urethane Casting
Covestro Baytec® 33965-1 Polyurethane

PTPU55 / 70911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.