MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Beryllium Copper, UNS C17300, TB00 Temper rod, bar, plate, tubing
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping.

Applications: springs, flexible metal hose, Bourdon tubing, bellows, clips, washers, retaining rings, and other parts subject to severe forming conditions but require high strength, anelasticity, and fatigue and creep resistance; in parts that require high strength or wear resistance along with good electrical conductivity and/or magnetic characteristics such as navigational instruments, non-sparking safety tools, firing pins, bushings, valves, pumps, shafts, and rolling mill parts.

TB00 temper rod, bar, plate, or tubing; all sizes.

Key Words: BeCu; CDA 173, ISO CuBe2Pb, CEN CW102C; Alloy M25
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³during age hardening, 2% max. decrease in length and 6% max. increase in density.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 45 - 8545 - 85
Tensile Strength, Ultimate 415 - 585 MPa60200 - 84800 psi
Tensile Strength, Yield 140 - 205 MPa20300 - 29700 psi
Elongation at Break 35 - 60 %35 - 60 %
Modulus of Elasticity 125 - 130 GPa18100 - 18900 ksi
Poissons Ratio 0.300.30
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa7250 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000091 - 0.000010 ohm-cm
@Temperature 20.0 °C
0.0000091 - 0.000010 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 20.0 - 100 °C
9.28 µin/in-°F
@Temperature 68.0 - 212 °F
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity  105 - 130 W/m-K
@Temperature 20.0 °C
729 - 902 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 130 - 133 W/m-K
@Temperature 200 °C
902 - 923 BTU-in/hr-ft²-°F
@Temperature 392 °F
Melting Point 865 - 980 °C1590 - 1800 °F
Solidus 865 °C1590 °F
Liquidus 980 °C1800 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 845 °C1550 °FHot-Shortness Temperature
Annealing Temperature 760 - 790 °C1400 - 1450 °F
Solution Temperature 760 - 790 °C1400 - 1450 °F
Aging Temperature 260 - 425 °C500 - 797 °F
Hot-Working Temperature 650 - 800 °C1200 - 1470 °F
Precipitation Temperature 316 °C
@Time 180 sec
600 °F
@Time 0.0500 hour
Air
Recrystallization Temperature 730 °C1350 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.8 - 2.0 %1.8 - 2.0 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 97 %97 %
Lead, Pb 0.20 - 0.60 %0.20 - 0.60 %
Other, total <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17200, TB00 Temper rod, bar, plate, tubing
Copper-Cobalt-Beryllium alloy, UNS C17500, TB00 Temper strip, rod, bar, plate, tubing, forged products
Beryllium Copper, UNS C17300, TD04 Temper rod, bar, plate, tubing, <9.5 mm
Beryllium Copper, UNS C17300, TH04 Temper rod, bar, plate, tubing, <9.5 mm
Copper-Cobalt-Beryllium alloy, UNS C17500, TF00 Temper strip, rod, bar, plate, tubing, forged products

MC17300c6 / 10843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.