MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-701 Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-101 is an ultra low molecular weight fluoroelastomer. At room temperature it is an opaque paste. At temperatures above 70°C (158 °F) it becomes a transparent, viscous fluid. DAI-EL® G-101 is not crosslinkable but is used as a plasticizer in other fluoroelastomers.

Typical Applications: Additive for other DAI-EL® fluoroelastomers. Mechanical property data shows effect of G-101 plasticizer on DAI-EL® G-701 Fluoroelastomer.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.76 - 1.77 g/cc1.76 - 1.77 g/ccDAI-EL® G-101
Viscosity 50 cP
@Temperature 60.0 °C
50 cP
@Temperature 140 °F
DAI-EL® G-101
Molecular Weight 3000 g/mol3000 g/molDAI-EL® G-101
Evaporation Loss 2.0 %
@Temperature 200 °C,
Time 7200 sec
2.0 %
@Temperature 392 °F,
Time 2.00 hour
DAI-EL® G-101
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656G-701, 33 PHR G101 added
 6666G-701, 0 PHR G101 added
 57
@Treatment Temp. 275 °C,
Time 259000 sec
57
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 33 PHR G101 added
 66
@Treatment Temp. 275 °C,
Time 259000 sec
66
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 0 PHR G101 added
Tensile Strength at Break 8.30 MPa1200 psiG-701, 33 PHR G101 added
 11.8 MPa1710 psiG-701, 0 PHR G101 added
 5.64 MPa
@Treatment Temp. 275 °C,
Time 259000 sec
818 psi
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 33 PHR G101 added
 8.85 MPa
@Treatment Temp. 275 °C,
Time 259000 sec
1280 psi
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 0 PHR G101 added
Elongation at Break 280 %280 %G-701, 0 PHR G101 added
 370 %370 %G-701, 33 PHR G101 added
 300 %
@Treatment Temp. 275 °C,
Time 259000 sec
300 %
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 0 PHR G101 added
 370 %
@Treatment Temp. 275 °C,
Time 259000 sec
370 %
@Treatment Temp. 527 °F,
Time 72.0 hour
After Air Aging, G-701, 33 PHR G101 added
100% Modulus  0.600 MPa
@Strain 100 %
87.0 psi
@Strain 100 %
G-701, 33 PHR G101 added
 1.80 MPa
@Strain 100 %
261 psi
@Strain 100 %
G-701, 0 PHR G101 added
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.80e+12 ohm-cm1.80e+12 ohm-cmDAI-EL® G-101
Dissipation Factor  0.0026
@Frequency 100 Hz
0.0026
@Frequency 100 Hz
DAI-EL® G-101
 0.080
@Frequency 100000 Hz
0.080
@Frequency 100000 Hz
DAI-EL® G-101
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.51 J/g-°C
@Temperature 80.0 °C
0.360 BTU/lb-°F
@Temperature 176 °F
DAI-EL® G-101
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.371.37DAI-EL® G-101
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 min
@Temperature 150 °C
0.333 hour
@Temperature 302 °F
Press cure, G-701
 1440 min
@Temperature 200 °C
24.0 hour
@Temperature 392 °F
Oven cure, G-701
 
Descriptive Properties
Test Formula100 phrRaw rubber (DAI-EL® G-701)
 3 phrMagnesium oxide
 6 phrCalcium hydroxide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sorbothane Polyurethane Damping Material, 50 Durometer
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-702 Fluoroelastomer
Covestro Baytec® MS-051 Polyurethane
Mearthane Durethane™ F DF-620A Closed Cell Foam Polyurethane
Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer

PDAIJ9872 / 209943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.