MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simple processing and good handling characteristics make V-376 an ideal alternative to BMI and polyimide resin systems. GC110 LM qualified specifications.

Key Features and Benefits:

  • Cyanate Ester resin provides outstanding electrical properties (Dk, Df)
  • Excellent Moisture resistance properties
  • Simplified handling and processing characteristics
  • Minimal degradation of mechanical properties in Hot/Wet environments
  • Self-Adhesive to many types of foam and honeycomb core

Applications/Qualifications:

  • Radomes
  • Reflectors
  • Antenna
  • Signature Control

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.5 %<= 1.5 %
Water Absorption 0.67 %0.67 %by weight; 14 day soak at 160°F
Thickness 0.127 microns0.00500 milcured laminate, per ply
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  427 MPa
@Temperature 149 °C
62000 psi
@Temperature 300 °F
0° Direction, Wet; ASTM D638
 648 MPa
@Temperature 23.9 °C
94000 psi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Tensile Modulus  23.4 GPa
@Temperature 23.9 °C
3400 ksi
@Temperature 75.0 °F
Dry; ASTM D638
 23.4 GPa
@Temperature 149 °C
3400 ksi
@Temperature 300 °F
Wet; ASTM D638
Flexural Strength 786 MPa
@Temperature 23.9 °C
114000 psi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D790
Flexural Modulus 22.8 GPa
@Temperature 23.9 °C
3300 ksi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D790
Compressive Strength  221 MPa
@Temperature 149 °C
32000 psi
@Temperature 300 °F
Dry; ASTM D695
 372 MPa
@Temperature 149 °C
54000 psi
@Temperature 300 °F
Wet; ASTM D695
 531 MPa
@Temperature 23.9 °C
77000 psi
@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus  22.8 GPa
@Temperature 23.9 °C
3300 ksi
@Temperature 75.0 °F
Dry; ASTM D695
 24.1 GPa
@Temperature 149 °C
3500 ksi
@Temperature 300 °F
Wet; ASTM D695
 24.1 GPa
@Temperature 149 °C
3500 ksi
@Temperature 300 °F
Dry; ASTM D695
Shear Strength 75.8 MPa
@Temperature 23.9 °C
11000 psi
@Temperature 75.0 °F
Short Beam; Dry; ASTM D2344
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.3
@Frequency 9.375e+9 Hz
3.3
@Frequency 9.375e+9 Hz
Dissipation Factor 0.0070
@Frequency 9.375e+9 Hz
0.0070
@Frequency 9.375e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C28.9 µin/in-°FZ-Axis
Glass Transition Temp, Tg 148 °C298 °FDMA; without post-cure
 178 °C352 °FDMA; with post-cure
 
Processing PropertiesMetricEnglishComments
Gel Time 3.00 - 30.0 min
@Temperature 135 °C
3.00 - 30.0 min
@Temperature 275 °F
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)288
Resin Flow (%)13-33325°F, 50psi
Resin Solids Content (%)35-41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
Huntsman AroCy XU 71787.07 L Cyanate Ester
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric
Huntsman AroCy XU 378 Cyanate Ester

PPARK080 / 89352

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.