MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATG s.r.l. CSM Chlorosulphonated Polyethylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 9040 - 90
Tensile Strength, Ultimate 12.0 - 24.0 MPa1740 - 3480 psi
Elongation at Break 150 - 500 %150 - 500 %
Rebound 5.0 - 20 %5.0 - 20 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -15.0 °C5.00 °F
 
Descriptive Properties
Abrasion Resistancemedium
Chemical Resistance to Animal and Vegetable Oils and Greasesmedium
Chemical Resistance to Aromatic Hydrocarbonslow
Chemical Resistance to Chloride Solventsnone
Chemical Resistance to Distilled Watermedium
Chemical Resistance to Ketoneslow
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C)high
Chemical Resistance to Medium-High Concentrated Acids (at 50°C)medium
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbonsmedium
Compression set at 100°Cmedium
Impermeability at gas (Oxygen and Nitrogen)medium
Resistance to Flamemedium
Resistance to Heat Agingmedium
Resistance to Low Temperatureslow
Resistance to Ozone and Weatheringhigh
Tear Strengthhigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chlorosulfonated Polyethylene Rubber (CM, CSM)
DuPont Mobility and Materials Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
DuPont Mobility and Materials Hypalon® 20 Chlorosulfonated Polyethylene Rubber, General Description
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene
DuPont Mobility and Materials Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, General Description

PATG012 / 79377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.