MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell A-C® 575P MAPE copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: Ethylene maleic anhydride copolymers in pastille form. The functionalization of a non polar polyethylene with 3% maleic anhydride, yielding a saponification (SAP) number of 35, provides the low molecular weight copolymer with non polar and polar characteristics, enough so that it can be emulsified and used in aqueous systems. The grafting of maleic anhydride provides polarity without polymer degradation, such as oxidation will. The maleic anhydride provides the ability to boost adhesion making it very suitable for adhesive applications. The low level of maleic anhydride, along with a patented Honeywell grafting process, aids thermal stability versus the competition and more highly maleated versions. Provides a boost in adhesion to paraffin based coatings for cardboard box coatings/saturants, providing increased moisture resistance and crush strength. It is used as a coupling agent for mineral or cellulosic filled composite systems.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
Brookfield Viscosity 4200 cP
@Temperature 140 °C
4200 cP
@Temperature 284 °F
 
Thermal PropertiesMetricEnglishComments
Dropping Point 106 °C223 °FMettler
 
Descriptive Properties
Hardness4.5 dmmASTM D5
Product FormPastille

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell A-C® 950P MAPP copolymer
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Honeywell A-C® 820A PE homopolymer
Honeywell A-C® 655 PE homopolymer Oxidized
Honeywell A-C® 617A PE homopolymer

PHONWL035 / 179580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.