MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0065 cm/cm0.0035 - 0.0065 in/in
Linear Mold Shrinkage, Transverse 0.0075 - 0.0105 cm/cm0.0075 - 0.0105 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi
Elongation at Break 2.0 %2.0 %
Tensile Modulus 7.80 GPa1130 ksi
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²
Coefficient of Friction, Dynamic 0.280.28
Coefficient of Friction, Static 0.320.32
K (wear) Factor 15.0 x 10-8 mm³/N-M7.45 x 10-10 in³-min/ft-lb-hr
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °F
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °F
Vicat Softening Point 170 °C
@Load 5.00 kg
338 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 230 °C410 - 446 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 70.0 - 90.0 °C
@Time 10800 sec
158 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LV-3H PA12-GF30
Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled
RTP Company RTP 205F HS  Nylon 12 (PA 12) Glass Fiber 30% - Heat Stable
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber
Polyram PlusTek PD305G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced

PLATH9897 / 177593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.