MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insulator in induction heat treating applications. RSLE-501`s very low thermal expansion coefficient and high hot strength combine to give it thermal shock resistance not found in other structural ceramic materials.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.10 g/cc0.0759 lb/in³
Porosity 31 %31 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787
Modulus of Rupture 0.0300 GPa4.35 ksiparallel to thickness
Compressive Yield Strength 48.0 MPa6960 psiat 2.7% consolidation parallel to thickness
Charpy Impact 1.08 J0.800 ft-lb
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.50e+9 ohm-cm7.50e+9 ohm-cmASTM D257-93
Dielectric Strength 1.69 kV/mm43.0 kV/inASTM D149-95
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.300 µm/m-°C
@Temperature 20.0 - 800 °C
0.167 µin/in-°F
@Temperature 68.0 - 1470 °F
Thermal Conductivity  0.550 W/m-K
@Temperature 200 °C
3.82 BTU-in/hr-ft²-°F
@Temperature 392 °F
parallel to thickness; ASTM C1113
 0.610 W/m-K
@Temperature 600 °C
4.23 BTU-in/hr-ft²-°F
@Temperature 1110 °F
parallel to thickness; ASTM C1113
 0.750 W/m-K
@Temperature 1000 °C
5.20 BTU-in/hr-ft²-°F
@Temperature 1830 °F
parallel to thickness; ASTM C1113
Shrinkage  0.10 %
@Temperature 800 °C,
Time 86400 sec
0.10 %
@Temperature 1470 °F,
Time 24.0 hour
 4.9 %
@Temperature 1100 °C,
Time 86400 sec
4.9 %
@Temperature 2010 °F,
Time 24.0 hour
 7.9 %
@Temperature 1100 °C,
Time 86400 sec
7.9 %
@Temperature 2010 °F,
Time 24.0 hour
Thickness
 
Component Elements PropertiesMetricEnglishComments
Other <= 0.30 %<= 0.30 %
SiO2 99.7 %99.7 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-200 Refractory Sheet
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite

CZRCI10 / 2873

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.