MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik Nisil Thermocouple Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: NISIL is the negative leg of thermocouple type N. This thermocouple is the most recent one among the different types covered by the international standards. It offers higher thermoelectric stability in air above 1000°C and better oxidation resistance than type E, J and K thermocouples. NISIL alloy cannot be exposed to sulphur-containing gases.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.585 g/cc0.3102 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 680 MPa
@Thickness 2.00 mm
98600 psi
@Thickness 0.0787 in
Tensile Strength, Yield 300 MPa
@Strain 0.2 %,
Thickness 2.00 mm
43500 psi
@Strain 0.2 %,
Thickness 0.0787 in
Elongation at Break 33 %
@Thickness 2.00 mm
33 %
@Thickness 0.0787 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000365 ohm-cm0.0000365 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 27.0 W/m-K
@Temperature 20.0 °C
187 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1420 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Magnesium, Mg 0.10 %0.10 %
Nickel, Ni 95.6 %95.6 %
Silicon, Si 4.3 %4.3 %
 
Descriptive Properties
emf, mV, Reference junction 0°C12.974; at 400°C
 16.748; at 500°C
 2.774; at 100°C
 20.613; at 600°C
 24.527; at 700°C
 28.455; at 800°C
 32.371; at 900°C
 36.256; 1000°C
 40.087; at 1100°C
 43.846; at 1200°C
 47.513; at 1300°C
 5.913; at 200°C
 9.341; 300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Nicrosil Thermocouple
Special Metals INCONEL® Alloy 600
Goodfellow T1-Thermocouple Alloy
Sandvik Iron Thermocouple
Thermal Ceramics 1302 Board and Shapes Molded Min-K Insulation

NSANDV103 / 18997

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.