MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant; Nylon 66, Heat Stabilized

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Moisture Absorption 1.50 %
@Temperature 23.0 °C
1.50 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inEurotec
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 9.00 GPa1310 ksiISO 527
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 290 °C518 - 554 °F
Feed Temperature 60.0 - 80.0 °C140 - 176 °FThroat
Mold Temperature 50.0 - 100 °C122 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.20 %<= 0.20 %ISO 960
Hold Pressure 50.0 - 100 MPa7250 - 14500 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ FH772 Polyamide 66, GF Reinforced, Flame Retardant
Ravago Manufacturing Americas Hylon® N1025HLFRA Nylon 66, 25% Glass Filled, Conditioned
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant

PEUROS037 / 147027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.