MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silver-bearing tough pitch Copper, UNS C11300
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: gaskets, radiators, busbars, windings, switches, chemical process equipment, clad metals, printed circuit foil.

Available as flat products, rod, wire, tube, and shapes.

Key Words: STP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 - 8.94 g/cc0.321 - 0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 221 - 455 MPa32100 - 66000 psi
Tensile Strength, Yield 69.0 - 365 MPa10000 - 52900 psiDepending on temper
Elongation at Break 55 %55 %in 101.6 mm (4 in.)
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.300.30Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000172 ohm-cm0.00000172 ohm-cm100% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 388 W/m-K
@Temperature 20.0 °C
2690 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1080 °C<= 1980 °F
Liquidus 1080 °C1980 °F
Annealing Point 482 - 760 °C900 - 1400 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99 - 99.9 %99 - 99.9 %
Oxygen, O <= 0.040 %<= 0.040 %
Silver, Ag <= 0.027 %<= 0.027 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphorus deoxidized Copper high residual phosphorus, UNS C12200
Copper, UNS C12000
Copper, UNS C12100
Phosphorus deoxidized arsenical Copper, UNS C14200
Silver-bearing tough pitch Copper, UNS C11400

MC11300d2 / 10585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.