MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik UNI-CAL® 866-1309 Colorant
Categories: Color; Other Engineering Material; Additive/Filler for Polymer

Material Notes: UNI-CAL® 866 Industrial Machine Colorants are closely controlled machine dispensable dispersions compatible with a variety of non-aqueous industrial and maintenance coatings. The broad compatibility range of these colorants allows the coatings manufacturer to reduce the number of special pigment dispersions normally required for tinting many special chemical coatings. The solvent in these colorants is a low aromatic, fast-evaporating, Rule 66-type solvent.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/cc
Density 1.35 g/cc0.0489 lb/in³
Solids Content 37.8 %37.8 %pigment
 41.3 %41.3 %vehicle
Volatile Organic Compounds (VOC) Content 284 g/l284 g/l
Volatiles 20.9 %20.9 %
 
Descriptive Properties
ColorantRaw Umber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik COLORTREND® PLUS™ 802-5511 Universal Machine Colorant
Evonik COLORTREND® 888-1045 Universal Machine Colorant
Evonik COLORTREND® 817-2032 Universal Machine Colorant
Evonik CHROMA-CHEM® 844-0352 Industrial Colorant
Evonik AQUATREND™ II 878-0837 In-Plant Colorant

PHUMB361 / 81363

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.