MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.

Data was collected by ISO methods and provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Water Absorption 0.10 %0.10 %
Moisture Absorption at Equilibrium 0.10 %0.10 %
Linear Mold Shrinkage, Flow 0.0055 cm/cm0.0055 in/in
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psi
Elongation at Break 25 %25 %
Elongation at Yield 1.9 %1.9 %
Tensile Modulus 1.90 GPa276 ksi
Charpy Impact Unnotched 16.0 J/cm²76.1 ft-lb/in²
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²
Tensile Creep Modulus, 1 hour 2000 MPa290000 psi
Tensile Creep Modulus, 1000 hours 1600 MPa232000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm1.00e+13 ohm
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
Dissipation Factor  0.00040
@Frequency 100 Hz
0.00040
@Frequency 100 Hz
 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
Comparative Tracking Index 575 V575 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C189 °F
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °F
Vicat Softening Point 89.0 °C192 °F
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe)
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe)
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe)
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe)

PSF197 / 66778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.