MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Bioline 316LVM Bar Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik Bioline 316LVM is a Molybdenum alloyed vacuum remelted stainless steel for the production of both temporary and permanent implants.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 160160Annealed
 155 - 210155 - 210Tube, thick wall, Bright annealed
 285285Bar, Wire, Medium tensile
 260 - 330260 - 330Tube, thick wall, Cold finished
 260 - 330260 - 330Profile, Cold rolled
 300300High tensile
Tensile Strength, Ultimate >= 490 MPa>= 71100 psiAnnealed
 490 - 690 MPa71100 - 100000 psiTube, thin wall, Annealed
 515 - 690 MPa74700 - 100000 psiTube, thick wall, Bright annealed
 >= 900 MPa>= 131000 psiBar, Wire, Medium tensile
 860 - 1100 MPa125000 - 160000 psiTube, thick wall, Cold finished
 860 - 1100 MPa125000 - 160000 psiProfile, Cold rolled
 860 - 1100 MPa125000 - 160000 psiTube, thin wall, Cold worked
 >= 1100 MPa>= 160000 psiHigh tensile
 >= 1400 MPa>= 203000 psiBar, Wire, Extra high tensile
Tensile Strength, Yield  190 MPa
@Strain 0.2 %
27600 psi
@Strain 0.2 %
Annealed
 >= 220 MPa
@Strain 0.2 %
>= 31900 psi
@Strain 0.2 %
Tube, thick wall, Bright annealed
 190 - 690 MPa
@Strain 0.2 %
27600 - 100000 psi
@Strain 0.2 %
Tube, thin wall, Annealed
 >= 690 MPa
@Strain 0.2 %
>= 100000 psi
@Strain 0.2 %
Tube, thin wall, Cold worked
 >= 690 MPa
@Strain 0.2 %
>= 100000 psi
@Strain 0.2 %
Tube, thick wall, Cold finished
 >= 690 MPa
@Strain 0.2 %
>= 100000 psi
@Strain 0.2 %
Profile, Cold rolled
 >= 700 MPa
@Strain 0.2 %
>= 102000 psi
@Strain 0.2 %
Bar, Wire, Medium tensile
 800 MPa
@Strain 0.2 %
116000 psi
@Strain 0.2 %
High tensile
Elongation at Break 12 %12 %Tube, thin wall, Cold worked
 >= 12 %>= 12 %Tube, thick wall, Cold finished
 12 %12 %Profile, Cold rolled
 12 %12 %High tensile
 15 %15 %Bar, Wire, Medium tensile
 40 %40 %Tube, thin wall, Annealed
 >= 45 %>= 45 %Tube, thick wall, Bright annealed
 45 %45 %Annealed
Modulus of Elasticity 200 GPa29000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
9.17 µin/in-°F
@Temperature 86.0 - 212 °F
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
0.116 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.025 %<= 0.025 %
Chromium, Cr 17.5 %17.5 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe 63.1 %63.1 %As Balance
Manganese, Mn 1.7 %1.7 %
Molybdenum, Mo 2.8 %2.8 %
Nickel, Ni 14 %14 %
Nitrogen, N <= 0.10 %<= 0.10 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.60 %0.60 %
Sulfur, S <= 0.0030 %<= 0.0030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medical Grade Stainless Steel 316LVM
AISI Type 316L Stainless Steel, annealed and cold drawn bar
Arcam Ti6Al4V Titanium Alloy
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked

NSANDV138 / 19032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.