MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® FC 23 UR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes:
  • clear and tinted grades for transparent applications
  • reinforced materials
  • Flame retardant and halogen free types
  • lubricated materials for added wear resistance

Mitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 0.35 %0.35 %Sim. to ISO 62
Viscosity Number 52 cm³/g0.52 dl/gLimiting Viscosity Number; ISO 1628-4
 58 cm³/g0.58 dl/g
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4
Melt Flow 8.4 g/10 min
@Load 1.20 kg,
Temperature 300 °C
8.4 g/10 min
@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 7 cm3/10min.; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ISO 2039-2
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1/-2
Elongation at Break >= 50 %>= 50 %ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %ISO 527-1/-2
Tensile Modulus 2.30 GPa334 ksiISO 527-1/-2
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 2.40 GPa348 ksiISO 178
Izod Impact, Notched (ISO) 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 180/4A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inIEC 60243-1
Dissipation Factor  0.00066
@Frequency 100 Hz
0.00066
@Frequency 100 Hz
IEC 60250
 0.0092
@Frequency 1e+6 Hz
0.0092
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VIEC 60112
 250 - 399 V250 - 399 VPLC 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
36.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 125 °C257 °FBall Pressure Temperature; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FISO 75-1/-2
Vicat Softening Point 148 °C298 °F50°C/h 50N; ISO 306
UL RTI, Electrical  130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact  125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL746B
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact  125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL746B
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
IEC 60695-11-20
Oxygen Index 35 %35 %ISO 4589-1/-2
Glow Wire Ignition Temperature  825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Descriptive Properties
Blow MoldingYes
Flame RetardantYes
Flame Retarding AgentYes
Heat Stabilized or Stable to HeatYes
High Impact or Impact ModifiedYes
Injection MoldingYes
Light Stabilized or Stable to LightYes
Release AgentYes
U.V. Stabilized or Stable to WeatherYes
Without FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 303-10 Polycarbonate Resin
Envalior Stanyl® TC153 PA46 FR(17), Dry, Flame Retardant, Heat Stabilized
Delrin Delrin® 500P NC010 POM
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant

PDSMEU622 / 31432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.