MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow AFFINITY™ EG 8200 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It exhibits excellent flow properties, exceptional heat aging and compression set when crosslinked, excellent weatherability. It is also effective in binder dispersions and as an impact modifier in polyolefins, exhibiting superior impact properties in blends with PE and PP.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Ratio I10/I2 = 7.1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575
Tensile Strength at Break 7.60 MPa1100 psi
Elongation at Break >= 1000 %>= 1000 %
100% Modulus 2.80 MPa
@Strain 100 %
406 psi
@Strain 100 %
Secant Modulus 0.0200 GPa2.90 ksi2% Secant Modulus
Tensile Set 0.00 %0.00 %Elongation set after break

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
Dow AFFINITY™ KC 8852 Polyolefin Elastomer
Dow AFFINITY™ SM 8400 Polyolefin Elastomer
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer

PDW252 / 34420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.