MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Thornel® T-50 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor  (discontinued **)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated to increase the interlaminar shear strength in a resin matrix composite.

6000 filaments/strand, 99+% carbon assay, 6.5 µm filament diameter, 2.75 m/g yield, 16 tpm twist (also available untwisted), 0.2 mm² fiber area in yarn cross section.

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Key Words: Carbon Fibre
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³
Specific Surface Area 0.45 m²/g0.45 m²/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2900 MPa421000 psi
Elongation at Break 0.60 %0.60 %
Tensile Modulus 390 GPa56600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000950 ohm-cm0.000950 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear -1.15 µm/m-°C
@Temperature 20.0 °C
-0.639 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 70.0 W/m-K486 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® T-650/42 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

ETHOR2 / 6074

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.