MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Ethylene Acrylic Acid
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 - 1.27 g/cc0.0329 - 0.0459 lb/in³Average value: 0.949 g/cc Grade Count:67
Water Absorption 0.0500 %0.0500 %Average value: 0.0500 % Grade Count:5
Moisture Absorption at Equilibrium 0.0500 %0.0500 %Average value: 0.0500 % Grade Count:5
pH 2.00 - 12.02.00 - 12.0Average value: 7.91 Grade Count:9
Viscosity 50.0 - 4000 cP50.0 - 4000 cPAverage value: 578 cP Grade Count:9
 575 - 30000 cP
@Temperature 140 - 190 °C
575 - 30000 cP
@Temperature 284 - 374 °F
Average value: 5530 cP Grade Count:12
Methyl Acrylate Content 6.50 - 20.0 %6.50 - 20.0 %Average value: 12.8 % Grade Count:8
Acrylic Acid Content 6.00 - 15.0 %6.00 - 15.0 %Average value: 8.09 % Grade Count:17
Thickness 60.0 microns2.36 milAverage value: 60.0 microns Grade Count:4
Melt Flow 0.500 - 1300 g/10 min0.500 - 1300 g/10 minAverage value: 59.2 g/10 min Grade Count:51
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000 - 2000.000 - 200Average value: 67.4 Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 62.0 - 85.062.0 - 85.0Average value: 73.3 Grade Count:4
Hardness, Shore D 22.0 - 50.022.0 - 50.0Average value: 40.2 Grade Count:6
Tensile Strength, Ultimate 1.50 - 24.7 MPa218 - 3580 psiAverage value: 14.9 MPa Grade Count:25
Film Tensile Strength at Yield, MD 8.10 - 9.40 MPa1170 - 1360 psiAverage value: 8.68 MPa Grade Count:4
Film Tensile Strength at Yield, TD 7.90 - 9.20 MPa1150 - 1330 psiAverage value: 8.32 MPa Grade Count:4
Tensile Strength, Yield 4.00 - 10.8 MPa580 - 1570 psiAverage value: 7.34 MPa Grade Count:21
Film Elongation at Break, MD 210 - 540 %210 - 540 %Average value: 433 % Grade Count:11
Film Elongation at Break, TD 440 - 750 %440 - 750 %Average value: 567 % Grade Count:11
Elongation at Break 50.0 - 800 %50.0 - 800 %Average value: 371 % Grade Count:29
Modulus of Elasticity 0.0221 - 0.124 GPa3.21 - 18.0 ksiAverage value: 0.0758 GPa Grade Count:15
Flexural Modulus 0.00500 - 0.0427 GPa0.725 - 6.20 ksiAverage value: 0.0222 GPa Grade Count:5
Secant Modulus, MD 0.0278 - 0.170 GPa4.03 - 24.7 ksiAverage value: 0.101 GPa Grade Count:7
Secant Modulus, TD 0.0271 - 0.175 GPa3.93 - 25.4 ksiAverage value: 0.0967 GPa Grade Count:7
Tensile Impact Strength 25.0 - 25.0 kJ/m²
@Temperature -40.0 - -40.0 °C
11.9 - 11.9 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 25.0 kJ/m² Grade Count:1
Elmendorf Tear Strength MD 255 - 450 g255 - 450 gAverage value: 346 g Grade Count:4
Elmendorf Tear Strength TD 305 - 510 g305 - 510 gAverage value: 429 g Grade Count:4
Elmendorf Tear Strength, MD 1.31 - 8.93 g/micron33.3 - 227 g/milAverage value: 5.27 g/micron Grade Count:11
Elmendorf Tear Strength, TD 5.10 - 30.2 g/micron130 - 767 g/milAverage value: 11.0 g/micron Grade Count:11
Dart Drop 6.56 - 11.8 g/micron167 - 300 g/milAverage value: 8.00 g/micron Grade Count:8
Dart Drop Test 4.30 - 7.90 g0.00948 - 0.0174 lbAverage value: 5.50 g Grade Count:3
Seal Strength 1800 - 2500 g/25 mm1800 - 2500 g/inAverage value: 2080 g/25 mm Grade Count:4
Film Tensile Strength at Break, MD 20.7 - 42.7 MPa3000 - 6190 psiAverage value: 30.6 MPa Grade Count:11
Film Tensile Strength at Break, TD 22.1 - 44.8 MPa3200 - 6500 psiAverage value: 30.3 MPa Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmAverage value: 1.00e+15 ohm-cm Grade Count:9
Dielectric Constant 2.30 - 2.802.30 - 2.80Average value: 2.48 Grade Count:5
Dissipation Factor 0.00700 - 0.01300.00700 - 0.0130Average value: 0.0102 Grade Count:5
 
Thermal PropertiesMetricEnglishComments
Melting Point 66.7 - 136 °C152 - 277 °FAverage value: 91.4 °C Grade Count:45
Vicat Softening Point 38.3 - 92.2 °C101 - 198 °FAverage value: 68.1 °C Grade Count:40
Dropping Point 76.0 - 105 °C169 - 221 °FAverage value: 95.1 °C Grade Count:12
 
Optical PropertiesMetricEnglishComments
Haze 3.00 - 18.3 %3.00 - 18.3 %Average value: 7.20 % Grade Count:8
Gloss 39.0 - 100 %39.0 - 100 %Average value: 62.5 % Grade Count:8
 
Processing PropertiesMetricEnglishComments
Processing Temperature 191 - 310 °C376 - 590 °FAverage value: 262 °C Grade Count:13
Nozzle Temperature 177 - 290 °C351 - 554 °FAverage value: 225 °C Grade Count:5
Adapter Temperature 180 - 300 °C356 - 572 °FAverage value: 229 °C Grade Count:8
Die Temperature 170 - 300 °C338 - 572 °FAverage value: 228 °C Grade Count:11
Melt Temperature 135 - 305 °C275 - 581 °FAverage value: 211 °C Grade Count:16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Appeel® 22D843 Ethylene Acrylate
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Overview of materials for Ethylene Butyl Acrylate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Arkema OREVAC® 18630 Maleic Anhydride Modified Ethylene - Acrylate Copolymer

O4192 / 77776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.