MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nordel® IP 5565 General Purpose Molding
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 5565 is an amorphous, high diene, EPDM grade designed for extruded applications requiring fast cure rates. It is ideally suited for continuously cured dense and sponge profiles. Molded applications will also benefit from the fast cure response, allowing shorter cycle times.

Information provided by manufacturer.

Key Words: 1155A18-06
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 74
@Temperature 100 °C
74
@Temperature 212 °F
ML 1 + 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6969Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 9.50 MPa1380 psiVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 383 %383 %Vulcanizate, Press cured, TC95 +3min at 160°C
50% Modulus 1.90 MPa
@Strain 50 %
1.90 MPa
@Strain 50 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 3.50 MPa
@Strain 100 %
508 psi
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 6.20 MPa
@Strain 200 %
899 psi
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 7.90 MPa
@Strain 300 %
1150 psi
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 30.8 kN/m176 pliDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 65 %
@Temperature 125 °C
65 %
@Temperature 257 °F
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -40.0 °C-40.0 °FTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5Sulfur
 0.5TMQ
 0.8DPTT
 0.8TMTD
 1.5ZnDBC
 1.5MBTS
 100Nordel® IP 5565
 125N774 Black
 5Zinc Oxide
 50Paraffinic Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4760P Compound
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber
Dow Nordel® IP 5565 ASTM D3568
Dow Nordel® IP 5565 Dense Extruded Profile
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured

PDVG44 / 34164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.