MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos R01A-01 Polypropylene Copolymer, Antistatic
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improved cycles. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Good stiffness and improved cycles
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.898 g/cc0.0324 lb/in³ASTM D1505
Melt Flow 1.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.7 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength, Ultimate 18.6 MPa2700 psi2 in/min.; ASTM D638
Tensile Strength, Yield 26.9 MPa3900 psi2 in/min (50 mm/min); ASTM D-638
Elongation at Break 550 %550 %2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 10 %10 %2 in/min.; ASTM D638
Modulus of Elasticity 0.669 GPa97.0 ksiASTM D638
Flexural Modulus, 1% Secant 896 MPa130000 psiASTM D790
Izod Impact, Notched 0.430 J/cm0.806 ft-lb/inASTM D256
Izod Impact, Unnotched >= 13.35 J/cm>= 25.01 ft-lb/inASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ProcessBlow Molding/Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Ineos N01N-00 Polypropylene Impact Copolymer
Ineos R01A-00 Polypropylene Random Copolymer
Ineos R01C-00 Polypropylene Random Copolymer

PSOLLN / 68269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.