MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retardants (non-furan emitting). It does not contain added antioxidants or metal deactivators. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • Recommended for applications requiring excellent ozone resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive – Flame Retardant Connectors and Seals
  • Electrical – Flame Retardant Connectors and seals; Flame Retardant Wire and Cable Jacket
Uses:
  • Automotive Applications
  • Cable Jacketing
  • Flexible Cord Jacketing
  • Wire & Cable Applications
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 98982 mm, 15 sec; ISO 868
Tensile Strength at Break 13.9 MPa2020 psiAcross Flow; ASTM D412
Tensile Stress at Strain 7.17 MPa
@Strain 100 %
1040 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 630 %630 %Across Flow; ASTM D412
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 31.1 kV/mm
@Thickness 2.03 mm
790 kV/in
@Thickness 0.0799 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical with Impact  85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL 746
 90.0 °C
@Thickness 3.00 mm
194 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 26 %26 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
ExxonMobil Santoprene® 251-85W232 Thermoplastic Elastomer
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer

PADVA126 / 22816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.