MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Impact Copolymer for Compounding and Injection Molded Applications

Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & garden products and appliances. It is characterized by its easy mold flow, excellent physical property balance of stiffness and impact at room temperature and sub ambient conditions as well as finished product dimensional stability.

Formolene® 2620A complies with the U. S. Food and Drug Administration regulation 21 CFR 177.1520(c)(3.4). This material may only be used in contact with foods of type I, II, III, IV-B, VI, VII, VIII and IX as described in Table 1 of 21 CFR 176.170(c)

Specimens were injection molded according to the conditions specified in ASTM D4101

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 20 g/10 min
@Temperature 230 °C
20 g/10 min
@Temperature 446 °F
I2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 17.9 MPa2600 psi2" (50mm) per min; ASTM D638
Elongation at Yield 5.0 %5.0 %2" (50mm) per min; ASTM D638
Flexural Modulus, 1% Secant 827 MPa120000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched  0.854 J/cm
@Temperature -30.0 °C
1.60 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 0.961 J/cm
@Temperature -18.0 °C
1.80 ft-lb/in
@Temperature -0.400 °F
ASTM D256
 1.07 J/cm
@Temperature 0.000 °C
2.00 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 5.87 J/cm
@Temperature 23.0 °C
11.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nexeo® HIVAL® 2620 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SG722 Polypropylene, Impact Modified; Molded/Extruded
M. Holland Company MTEGRITY™ CP510 Polypropylene Copolymer
Total PPC 9712 Polypropylene, Heterophasic Copolymer
ExxonMobil Exceed™ PP7815E1 Polypropylene Homopolymer

PFPCPQ017 / 150249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.