System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Aurora Plastics TufTech™ GA-3188AHP PVC Compound
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
Material Notes:
Application: RoHS compliant, phthalate free, 105°C flame retardant jacketing material suitable for extrusion applications.
Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.26
g/cc
1.26
g/cc
ASTM D792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
88
@Time 15.0 sec
88
@Time 0.00417 hour
ASTM D2240
Tensile Strength
19.3
MPa
2800
psi
ASTM D412
20.458
MPa
@Temperature 100 °C,
Time 14400 sec
2967.2
psi
@Temperature 212 °F,
Time 4.00 hour
Oil Aged
Elongation at Break
300 %
300 %
ASTM D412
>= 234 %
@Treatment Temp. 100 °C,
Time 14400 sec
>= 234 %
@Treatment Temp. 212 °F,
Time 4.00 hour
Oil Aged
Abrasion
80
@Load 1.00 kg
80
@Load 2.20 lb
Taber, H18 Wheel; ASTM D4060
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-20.0
°C
-4.00
°F
ASTM D746
Flammability, UL94
V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Oxygen Index
27.5 %
27.5 %
ASTM D2863
Processing Properties
Metric
English
Comments
Processing Temperature
174
-
185
°C
345
-
365
°F
Suggested Stock
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aurora Plastics GA-7056D-FR-105 PVC
Karina 85/201-DA-IS-SI-AT Clear PVC Compound
Karina E 85/201-DA-IS-SI Clear PVC Compound
Karina E 85/201-DA-IS-SI-AT Clear Crystal PVC Compound
Armacell ArmaSport® MFC-2 Continuous Rolls, PVC/NBR
PSEPN074 / 179078
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.