Hostacom G3 R05 2003 is a 30% glass fiber reinforced PP homopolymer, with excellent stiffness, good dimensional stability and low creep under load at elevated temperatures. Product is available as non color matched, black, pellet form. Applications: Structural PartsInformation provided by LyondellBasell. |