MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adstif HA 801U Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA801U very high melt flow, nucleated polypropylene homopolymer is available in pellet form.  This resin is typically used in high-speed injection molding of thin-walled parts, and as a building block for compounded applications that require high flow and high stiffness. Application: Color Concentrates; Polymer Modifier; TWIM Food Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D 792
Melt Flow 65 g/10 min
@Load 2.16 kg,
Temperature 230 °C
65 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psi50mm/min; ASTM D 638
Elongation at Yield 6.0 %6.0 %ASTM D 638
Flexural Modulus, 1% Secant 2000 MPa290000 psiProcedure A, 1.3 mm/min; ASTM D 790
Izod Impact, Notched 0.160 J/cm
@Temperature 23.0 °C
0.300 ft-lb/in
@Temperature 73.4 °F
Method A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodCompounding; Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adstif HA 899J Polypropylene
LyondellBasell Adstif HA 5029 Polypropylene
LyondellBasell Adstif HA 849K Polypropylene
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
A. Schulman Diamond NPP30-2000HC Homopolymer Polypropylene

PEQT7020 / 218659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.