MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY black 9205 is especially suitable for injection molded parts in automotive applications being in long term contact with coolants (water/glycol mixtures). Polymer designation Acc. to ISO: PA 6T/6I. Acc. to ASTM: PPA, polyphthalamide The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT is suitable for production of technical parts in the application fields of:
  • Electro
  • Electronics
  • Automotive
  • Safety technology
  • Mechanical engineering
  • Domestic appliances

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³Dry; ISO 1183
Water Absorption 3.5 %3.5 %Sim. to ISO 62
Moisture Absorption 1.80 %1.80 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 270 MPa39200 psiConditioned; ISO 2039-1
 280 MPa40600 psiDry; ISO 2039-1
Tensile Strength at Break 170 MPa24700 psiConditioned; ISO 527-1/-2
 190 MPa27600 psiDry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %Dry; ISO 527-1/-2
 2.0 %2.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 11.0 GPa1600 ksiDry; ISO 527-1/-2
 11.0 GPa1600 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmDry; IEC 60093
 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 30.0 kV/mm762 kV/inDry; IEC 60243-1
 30.0 kV/mm762 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 575 V575 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 325 °C617 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C302 °FLong Term; ISO 2578
 270 °C518 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °C311 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveCooling and climate control
 Exterior
 Interior
 Powertrain and Chassis
FormGranules
Industry & Consumer goodsHeating systems
 Hydraulics & Pneumatics
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsImproved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® HTN51G35HSL BK083 PA6T/XT-GF35
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Celanese Hostaform® C 9021 POM, Unfilled
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40

PGRH370 / 157079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.