MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Texin® 945U Urethane Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Key Features:
  • Unfilled
  • U.V. stabilized or stable to weather

Suitable processing methods:

  • Injection molding
  • Profile extrusion
  • Sheet extrusion

Information provided by Bayer Polymers.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress at Strain 33.0 MPa
@Strain 50 %
4790 psi
@Strain 50 %
Elongation at Break >= 50 %>= 50 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 160 µm/m-°C
@Temperature 20.0 °C
88.9 µin/in-°F
@Temperature 68.0 °F
Vicat Softening Point 116 °C241 °F50°C/h 50N
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 °C401 °FInjection Molding
Mold Temperature 35.0 °C95.0 °FInjection Molding
Injection Pressure 45.0 MPa6530 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 950 Urethane Thermoplastic Elastomer
Covestro Texin® 950U Urethane Thermoplastic Elastomer
Covestro Texin® 185 Urethane Thermoplastic Elastomer
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
Covestro Texin® 390 Urethane Thermoplastic Elastomer

PB10323 / 26361

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.