MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Avient Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 6.88 g/cc6.88 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 6.89 MPa999 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 1.0 %1.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 4.03 GPa585 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 12.4 MPa1800 psiASTM D790
Flexural Modulus 2.69 GPa390 ksiASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.993 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched (ISO) 5.25 kJ/m²2.50 ft-lb/in²ASTM D256
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 271 °C450 - 520 °F
Mold Temperature 37.8 - 48.9 °C100 - 120 °F
Drying Temperature 71.1 °C160 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
FeaturesNon-Toxic
FormsPellets
Generic MaterialPEBA-Ether
Generic NamePolyether Block Amide (PEBA-Ether)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesIndustrial Applications
 Medical/Healthcare Applications
 Projectiles
 Radiation Shielding
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ecomass® 1002ZB92 Filled PEBA, Extrusion/Injection Molding Grade
Evonik Vestamid® E40-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Evonik Vestamid® X4442 nf (dry properties) Polyether Block Amide (PEBA)
Arkema Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)
RTP Company RTP 2999 X 125934 A NS Polyether-Block-Amide (PEBA / COPA); Barium Sulfate Filled

PH0POL1292 / 145861

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.