MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Key Words: TPU Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Hardness, Shore D 4747ASTM D2240
Tensile Strength, Ultimate 36.0 MPa5220 psiASTM D412
Tensile Stress at Strain  12.0 MPa
@Strain 100 %
1740 psi
@Strain 100 %
ASTM D-412
 21.0 MPa
@Strain 300 %
3050 psi
@Strain 300 %
ASTM D-412
Elongation at Break 490 %490 %ASTM D412
Modulus of Elasticity 0.0650 GPa9.43 ksi
Shear Modulus 0.0390 GPa5.66 ksi
Tear Strength 140 kN/m799 pliASTM D624
Taber Abrasion, mg/1000 Cycles 5555H-18 wheel; ASTM D-1044.
Tensile Set 65 %65 %at break; ASTM D-412
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+11 ohm-cm>= 1.00e+11 ohm-cmDIN 53482/VDE 0303
Surface Resistance >= 1.00e+11 ohm>= 1.00e+11 ohmDIN 53482/VDE 0303
Comparative Tracking Index >= 600 V>= 600 VDIN/IRC 112
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 130 °C266 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer

PSF982 / 67198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.