MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C42500, OSO25 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, piercing, forming and drawing.

Applications: electrical switches, springs, terminals, connectors, fuse clips, pen clips, weather stripping.

Test specimen: flat products - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.78 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 7272
Hardness, Rockwell 30T 3636Hardness, HR30T
Tensile Strength, Ultimate 315 MPa45700 psi
Tensile Strength, Yield  125 MPa
@Strain 0.2 %
18100 psi
@Strain 0.2 %
 125 MPa
@Strain 0.5 %
18100 psi
@Strain 0.5 %
Elongation at Break 48 %48 %in 50 mm
Modulus of Elasticity 110 GPa16000 ksiHard
 125 GPa18100 ksiAnnealed
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
0.00000620 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.4 µm/m-°C
@Temperature 20.0 - 100 °C
10.2 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 120 W/m-K
@Temperature 20.0 °C
833 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1010 - 1030 °C1850 - 1890 °F
Solidus 1010 °C1850 °F
Liquidus 1030 °C1890 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 700 °C797 - 1290 °F
Hot-Working Temperature 790 - 840 °C1450 - 1540 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 87 - 90 %87 - 90 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.35 %<= 0.35 %
Tin, Sn 1.5 - 3.0 %1.5 - 3.0 %
Zinc, Zn 9.5 %9.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C42200, H02 Temper flat products
Copper, UNS C41500, H03 Temper flat products
Copper, UNS C40800, H08 Temper flat products
Copper, UNS C27000 (Yellow brass), H02 Temper wire
Copper, UNS C26800 (Yellow brass), OSO15 Temper flat products

MC42500b3 / 11324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.