MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-37063 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-37063 is a specialty thermoplastic elastomer specifically designed for medical and healthcare industry. Medalist MD-37063 is a translucent, medium hardness, lubricated grade that can be sterilized and exhibits excellent adhesion to ABS, PC/ABS, and PC.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Bondability; Good Sterilizability; Medium Density; Medium Hardness

Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Melt Flow  2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 30 g/10 min
@Load 5.00 kg,
Temperature 210 °C
30 g/10 min
@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240
 63
@Time 5.00 sec
63
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 8.96 MPa1300 psiASTM D412
Tensile Stress at Strain 4.48 MPa
@Strain 300 %
650 psi
@Strain 300 %
ASTM D412
Elongation at Break 600 %600 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 127 - 149 °C260 - 300 °F
Middle Barrel Temperature 138 - 160 °C280 - 320 °F
Front Barrel Temperature 149 - 171 °C300 - 340 °F
Nozzle Temperature 171 - 193 °C340 - 380 °F
Melt Temperature 171 - 193 °C340 - 380 °F
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Apec® 1745 Polycarbonate
Teknor Apex Medalist® MD-50133 Thermoplastic Elastomer
Teknor Apex Medalist® MD-36048 Thermoplastic Elastomer
Teknor Apex Medalist® MD-34065 Thermoplastic Elastomer
Teknor Apex Medalist® MD-34060 Thermoplastic Elastomer

PTEKNQ0725 / 237216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.