MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Pin Red Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Quercus Palustris; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.580 g/cc0.580 g/ccGreen, based on volume
 0.630 g/cc0.630 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4760 N1070 lb (f)Green
 6717 N1510 lb (f)12% moisture content
Tensile Strength at Break 5.52 MPa800 psiGreen, perpendicular to grain
 7.24 MPa1050 psi12% moisture content, perpendicular to grain
Modulus of Elasticity 9.10 GPa1320 ksiGreen
 11.9 GPa1730 ksi12% moisture content
Modulus of Rupture 0.0572 GPa8.30 ksiGreen
 0.0965 GPa14.0 ksi12% moisture content
Compressive Strength 4.96 MPa720 psiGreen, perpendicular to grain
 7.03 MPa1020 psi12% moisture content, perpendicular to grain
 25.4 MPa3680 psiGreen, parallel to grain
 47.0 MPa6820 psi12% moisture content, parallel to grain
Shear Strength 8.89 MPa1290 psiGreen, parallel to grain
 14.3 MPa2080 psi12% moisture content, parallel to grain
Impact 4545Impact bending in inches, 12% moisture content
 4848Impact bending in inches, green
Work to Maximum Load 0.0965 J/cm³14.0 in-lb/in³Green
 0.102 J/cm³14.8 in-lb/in³12% moisture content
 
Thermal PropertiesMetricEnglishComments
Shrinkage 4.3 %4.3 %Radial, from green to oven dry, US origin
 9.5 %9.5 %Tangential, from green to oven dry, US origin
 14.5 %14.5 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cherrybark Red Oak Wood
Laurel Red Oak Wood
Scarlet Red Oak Wood
Willow Red Oak Wood
Water Red Oak Wood

PTSU033 / 71475

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.