MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® Tite 335AF Skin packing / heat seal coating  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Skin packing / heat seal coating

Usage: Michem® Tite 335AF is a coating which bonds corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product in between. Adhesion to most water based or litho inks is excellent, but the inks must be wax-free. This product is hot melt gluable.

Application Data: Michem® Tite 335AF should be applied to sheeted corrugated using a roll coater.

Typical uses include: Displays; Parts packs and Shipping protection

Food Contact Information when manufactured in the USA:
FDA:
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 - 0.990 g/cc0.970 - 0.990 g/cc
pH 7.8 - 8.87.8 - 8.8
Brookfield Viscosity 150 - 850 cP150 - 850 cPSpindle # 3, rpm 60
Viscosity Measurement 20 - 4520 - 45[sec], EZ cup, Cup # 3
 
Descriptive Properties
AppearanceSemi-viscous liquid
Solids TypePolymer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion
Michelman® Michem® Tite 242AF Skin packaging primer
Momentive Performance Materials AC6091 Boron Nitride (BN) Powder

WMICHEL167 / 135084

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.