Flame High light reflection grade, Anti-environmental pollution type (Non-Bromine / non-phosphorus type), flame resistant grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: Flame retardant, high reflectivity. Uses: LEDs, Light Application, Reflectors. Appearance: White. Forms: pellets. Processing Method: Injection Molding.Information provided by Teijin Chemicals Ltd. |