MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ceramic Process Systems AlSiC-8, 70 vol% SiC
Categories: Metal; Metal Matrix Composite

Material Notes: Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.

CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, components can be plated using conventional plating schemes to allow for assembly and integration operations. The CPS fabrication process provides a material that has a unique combination of physical properties: a compatible CTE, high thermal conductivity, light weight, and tight dimensional tolerance without machining (i.e. net-shape).

Information provided by Ceramic Process Systems.

Key Words: Aluminum Silicon Carbide Metal Matrix Composites; CPS; MMC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.99 g/cc0.108 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 217.5 GPa31550 ksiYoung's Modulus
Poissons Ratio 0.1540.154
Fracture Toughness 11.67 MPa-m½10.62 ksi-in½
Shear Modulus 94.2 GPa13700 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.60 µm/m-°C
@Temperature 30.0 °C
3.67 µin/in-°F
@Temperature 86.0 °F
 9.00 µm/m-°C
@Temperature 250 °C
5.00 µin/in-°F
@Temperature 482 °F
Specific Heat Capacity 0.741 J/g-°C0.177 BTU/lb-°F
Thermal Conductivity 180 W/m-K1250 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceramic Process Systems AlSiC-9, 63 vol% SiC
Ceramic Process Systems AlSiC-10, 54 vol% SiC
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
PCC-Advanced Forming Technology 30% AlSiC Metal Matrix Composite
DWA 6092/SiC/25p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Extruded

NZMAL0 / 20023

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.