MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec 975 Alumina, 99.5%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: 975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high density, superior wear resistance, and moderate flexural strength. Another advantage is its highly uniform white color compared to conventional 99.5% aluminas. The material’s white color remains consistent under either reducing or oxidizing conditions. It can be used for ballistic protection and ceramic armor.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %0.00 %DIN EN 623-2 / ASTM-C373
Particle Size 2.0 - 3.0 µm2.0 - 3.0 µmMedian Grain (d50)
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 17001700HV 0.5; DINV ENV 843-4
Tensile Strength at Break 172 MPa24900 psiACMA Test #4 / DIN EN 843-1
Tensile Modulus 380 GPa55100 ksiYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 310 MPa45000 psi20 x 40 mm
Compressive Strength 2400 MPa348000 psiASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.300.30DINV ENV 843-2
Fracture Toughness 4.00 MPa-m½3.64 ksi-in½DIN 51109
Shear Modulus 131 GPa19000 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM-D257
Dielectric Constant 10
@Frequency 1e+6 Hz
10
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength 7.874 kV/mm200.0 kV/in6.35 mm (1/4") IEC 672-1
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
0.00010
@Frequency 1e+6 Hz
Dielectric Loss Index 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.30 µm/m-°C4.06 µin/in-°FDIN EN 821-1
 5.60 µm/m-°C
@Temperature 20.0 - 200 °C
3.11 µin/in-°F
@Temperature 68.0 - 392 °F
 7.00 µm/m-°C
@Temperature 20.0 - 600 °C
3.89 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C373
 8.00 µm/m-°C
@Temperature 20.0 - 1000 °C
4.44 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.900 J/g-°C
@Temperature 100 - 200 °C
0.215 BTU/lb-°F
@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 35.4 W/m-K246 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1530 °C2790 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.5 %99.5 %
 
Descriptive Properties
ColorWhite
Thermal Shock Resistance R1 (K)225Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec RK 87 Alumina, 99.8%
CeramTec 433 Alumina, 99.9%
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
CeramTec 614/698 Alumina, 96%

CCERA932 / 107532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.