MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Pyrotek Pyrite Vacuum Formed Product
Categories: Ceramic

Material Notes: Off White Color

Applications

  • Tap hole cones
  • Riser sleeves
  • Launder insulation
  • Head boxes
  • Ladle lining
  • Pouring cups

Advantages

  • Good thermal shock resistance
  • High strength/weight ratio
  • Low thermal conductivity
  • Non wetting

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.250 g/cc0.00903 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1260 °C2300 °F
Shrinkage 4.0 %
@Temperature 1260 °C,
Time 86400 sec
4.0 %
@Temperature 2300 °F,
Time 24.0 hour
Linear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VTS 243FR Epoxy Syntactic-Core Film
Rogers Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
Morgan Advanced Ceramics Inorganic RCF Vacuum Formed Products I-2100 Thermal Ceramic

CPYRO038 / 1800

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.