MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® SEG7 35% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Ultramid SEG7 is a 35% glass reinforced, injection molding type 6 nylon requiring high strength, surface aesthetics, and good processability. This product has excellent surface appearance while maintaining a good balance of physical properties, such as high strength, improved toughness, and chemical resistance. It features superior flow properties, and is suited for parts having thinner walls and those requiring long lengths. It shows lower pressure, temperature, and cycle time requirements than conventional grades.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 1.0 %1.0 %24 hour; ISO Test
 6.3 %6.3 %ISO 62
Moisture Absorption at Equilibrium 1.7 %1.7 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM Test
Tensile Strength at Break 185 MPa26800 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 185 MPa26800 psi5mm/min; ISO 527
Elongation at Break 3.5 %3.5 %5mm/min; ISO 527
 3.5 %3.5 %0.2 in/min; ASTM Test
Flexural Strength 290 MPa42100 psiASTM Test
Flexural Modulus 9.67 GPa1400 ksiASTM Test
Izod Impact, Notched 1.50 J/cm
@Thickness 3.17 mm
2.81 ft-lb/in
@Thickness 0.125 in
ASTM Test
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Flammability, UL94 HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (DAM)
BASF Capron® SEG7 35% Glass-Filled Nylon 6 (Dry)
ExxonMobil Label-Lyte™ 50TD200 OPP Film
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM)
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)

PBASF9387 / 85151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.