MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Sanitary gaskets made from Fluoraz® 890 are ideal for use in standard SIP and CIP applications where EPDMs and FKMs fail. While EDPMs and FKMs can provide a deal for extended periods, changes in physical properties can have adverse effects beyond simple volume swell. A decrease in hardness or drop in modulus signals a reduction in compressive strength. If a sanitary gasket is retorqued to the installations specification, the gasket will be compressed at a greater level than desired, resulting in increased intrusion into the process stream. An increase in hardness/modulus and a drop in elongation means embrittlement. The seal will be undertorqued, resulting in either leaks or cracking.

Fluoraz 890 is formulated for use in sanitary gaskets where both USP and FDA compliance is required, making it an excellent compound for both pharmaceutical and other hygienic fluid handling applications such as seals for brewery applications. Fluoraz 890 metal and TOC extractables are an order of magnitude lower than premium competitive FKM formulations, ensuring little or no contamination into the process stream. Fluoraz 890 also meets the extractive requirements of both 21 CFR 177.2600 (e), (f) and 21 CFR 177.2400 (d) extraction testing for perfluoroelastomers. Fluoraz 890 sanitary gaskets by Greene Tweed are designed for minimal intrusion.

Fluoraz 890 is also available in O-rings and custom shapes where a medium durometer hardness is desired.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.65 g/cc1.65 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 17.9 MPa2600 psiASTM D1414
Tensile Strength, Yield 5.86 MPa850 psi@50% Elongation; ASTM D1414
 11.7 MPa1700 psi@100% Elongation; ASTM D1414
Elongation at Break 175 %175 %ASTM D1414
Compression Set 30 %
@Temperature 204 °C,
Time 252000 sec
30 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -5.00 °C23.0 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering E80Q Ethylene Propylene Rubber
Dow Nordel® IP 4520 Molded Brake Part
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer

PGREEN44 / 42338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.