MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow CYRACURE™ UVR-6110 Cycloaliphatic Epoxide
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard base resin. It is useful in many applications in which low viscosity is not required:
  • Metal decoration coatings
  • Overprint varnishes

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.167 - 1.182 g/cc1.167 - 1.182 g/cc
Viscosity 350 - 450 cP350 - 450 cP
Maximum Moisture Content 0.0500.050wt% water
ASTM Color 0.00 - 1000.00 - 100PtCo
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.00 - 0.100.00 - 0.10Acidity, wt%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow CYRACURE™ UVR-6128 Cycloaliphatic Epoxide
Dow BETAMATE™ 1045 Epoxy
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide
DuPont Mobility and Materials Betamate™ 1496V Epoxy Adhesive, Body Shop Grade
Dow BETAMATE™ 7000/7050 L Epoxy

PDOW1045 / 30249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.