MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LL 8450.31 Rotational Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require the optimum balance of stiffness and processability.

Availability: Latin America, North America and South America

Additive:

  • Stabilizer: Yes
  • Long Term UV-8
Applications:
  • Consumer Articles
  • Junction Boxes
  • Playground Equipment
  • Potable Water Tanks
  • Small Storage Boxes
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D4883
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D1693
ESCR 10% Igepal® 185 hour185 hourASTM D1693
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.9 MPa2600 psi2.0 in/min; ASTM D638
Elongation at Yield 20 %20 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 758 MPa110000 psiASTM D790
Impact Test  77.3 J
@Thickness 3.17 mm,
Temperature -40.0 °C
57.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM
 183 J
@Thickness 6.35 mm,
Temperature -40.0 °C
135 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C261 °FASTM D3418
Crystallization Temperature 112.3 °C234.1 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °C142 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C100 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LL 8360.29 Rotational Molding Resin
Braskem ML3601U LLDPE Rotomolding Polyethylene
ExxonMobil LL 8460.29 Rotational Molding Resin
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer
ExxonMobil LLP8555.25 Rotational Molding Resin

PEXB232 / 37537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.