MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Manganese Brass, UNS C66700
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Good to excellent corrosion resistance. Excellent cold formability. Fabricated by blanking, bending, forming, stamping, welding.

Applications: brass products, resistance welded by spot, seam, and butt welding.

Available as flat products and wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.53 g/cc0.308 lb/in³Value for UNS C26000
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 315 - 689 MPa45700 - 99900 psi
Tensile Strength, Yield 83.0 - 683 MPa12000 - 99100 psiDepending on temper
Elongation at Break 60 %60 %in 50.8 mm.
Tensile Modulus 110 GPa16000 ksi
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000101 ohm-cm0.0000101 ohm-cm17% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 - 300 °C
11.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 8.07 W/m-K56.0 BTU-in/hr-ft²-°F
Melting Point 1050 - 1090 °C1920 - 2000 °F
Solidus 1050 °C1920 °F
Liquidus 1090 °C2000 °F
Annealing Point 499 - 704 °C930 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 727 - 849 °C1340 - 1560 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 70 %70 %
Manganese, Mn 1.2 %1.2 %
Zinc, Zn 28.8 %28.8 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Manganese Bronze A, UNS C67500
Aluminum Brass Arsenical, UNS C68700
Forging Brass, UNS C37700
Manganese Brass, UNS C67300

MC66700b1 / 11679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.