MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Protectosil® AQUA-TRETE® 20 Surface Treatment
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product Description: A clear, penetrating, waterborne, breathable water repellent for use on concrete and masonry. Ready-to-use, low-VOC, silane emulsion. Reduces the ingress of water an waterborne contaminates that cause premature deterioration of the substrate. Penetrates the substrate and chemically bonds with silica to form a permanent attachment of the water repellent molecule. Protectosil AQUA-TRETE 20 water repellent is especially suited for application when solvent-borne products are not acceptable, as in states that have VOC regulations for AIM coatings. Protectosil AQUA-TRETE 20 meets all national and state VOC regulations. By preventing water and waterborne contaminates from entering the substrate, Protectosil AQUA-TRETE 20 reduces such problems are efflorescence, leaching, acid rain deterioration, scaling, dirt buildup, staining, corrosion of reinforcing steel mildew. Treated surfaces are fully breathable because their natural moisture vapor transmission is not affected. This will reduce problems that entrapped moisture can cause, including blushing of the sealer and freeze-thaw damage.

Applications: For use on concrete to protect the reinforcing steel from corrosion due to the effects of water, deicing salts and other waterborne chemicals. Protects precast concrete (including GFRC) from the damaging effects of acid rain and freeze-thaw cycles. Keeps concrete clean by reducing the amount of dirt and other pollutants that it may absorb. Some denser concrete masonry units (split-face, fluted or ground-face blocks) and pavers can also be protected from water absorption. Other suitable substrates include brick masonry, sandstone, terra-cotta, hand molded bricks and some natural stones.

Advantages: Protectosil AQUA-TRETE 20 is a silane/siloxane blend in a proprietary emulsion system. Unlike other silane or siloxane emulsion systems. Protectosil AQUA-TRETE 20 is ready to use and is suitable for concrete and brick masonry, without the need to blend oils, silicones, sterates or acrylates into the system. Protectosil AQUA-TRETE 20 is designed to provide a high level of repellency with penetration. The active components are unique because they chemically bond to the silica in the substrate and set up a hydrophobic layer of protection. By incorporating Protectosil AQUA-TRETE 20 into your integrated design, you can earn vital Leadership in Energy & Environmental Design (LEED) credits for both new and existing construction projects. The main benefits of the product are:

  • Non flammable
  • Excellent resistance to chloride ion ingress
  • Reduced efflorescence
  • Breathable system
  • Good penetration into substrate
  • No change in surface appearance
  • High resistance to alkali attack
  • Long service life
  • Substrates already treated with Protectosil AQUA-TRETE 20 can be painted over
  • Keeps substrates cleaner

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.995 g/cc0.0359 lb/in³
Volatile Organic Compounds (VOC) Content 90 g/l90 g/l
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.3 °C>= 200 °F
 
Descriptive Properties
Coloremulsion
Content20%active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Concrete, clinker aggregate
Evonik Inhibitors MVC
Wacker Wacker® EE 180206 Silicone Fluid Emulsion
Evonik Protectosil® AQUA-TRETE® BHN Surface Treatment
Evonik Protectosil® 300S Surface Treatment

PEVONIM120 / 197324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.