MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom HBG 479R BLACK Polypropylene with 30% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Hostacom HBG 479R BLACK is a 30% glass fiber reinforced PP homopolymer, with low flowability, very good LTHS (long term heat stability) and high rigidity. During the production process an enlarged testing plan is used because of the customer application "pedal support". The product is available in black color, pellet form. Applications: Automotive Parts

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183-1A
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527-1,-2
Elongation at Break 3.0 %3.0 %ISO 527-1,-2
Tensile Modulus 6.80 GPa986 ksiISO 527-1,-2
Flexural Modulus 7.00 GPa1020 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched  5.20 J/cm²
@Temperature 0.000 °C
24.7 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eU
 5.40 J/cm²
@Temperature 23.0 °C
25.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1/1eA
 1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
ISO 179-1/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ FR 8000 Polypropylene with 30% Glass Fiber
LyondellBasell Hostacom G3 N01 L Polypropylene with 30% Glass Fiber Filler
LyondellBasell Hostacom TKG 324N BLACK Polypropylene with 30% Glass Fiber Filler
Avient Edgetek® PPX-30GF/000 HI Copolymer Propylene - Chemically Coupled - 30% Glass Fiber
Albis Plastics Polypropylene A 12 H-GF30 C-1 30% Glass Fiber

PEQT7963 / 219600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.